http://scholars.ntou.edu.tw/handle/123456789/23600
DC 欄位 | 值 | 語言 |
---|---|---|
dc.contributor.author | Tai, Cheng-Ling | en_US |
dc.contributor.author | Tai, Po-Jui | en_US |
dc.contributor.author | Hsiao, Ting-Jung | en_US |
dc.contributor.author | Chiu, Po-Han | en_US |
dc.contributor.author | Tseng, Chien-Yu | en_US |
dc.contributor.author | Tsao, Tzu-Ching | en_US |
dc.contributor.author | Chung, Tsai-Fu | en_US |
dc.contributor.author | Yang, Yo-Lun | en_US |
dc.contributor.author | Chen, Chih-Yuan | en_US |
dc.contributor.author | Wang, Shing-Hoa | en_US |
dc.contributor.author | Yang, Jer-Ren | en_US |
dc.date.accessioned | 2023-02-15T01:17:31Z | - |
dc.date.available | 2023-02-15T01:17:31Z | - |
dc.date.issued | 2022-10-01 | - |
dc.identifier.uri | http://scholars.ntou.edu.tw/handle/123456789/23600 | - |
dc.description.abstract | The effects of natural ageing treatment prior to artificial ageing treatment on the microstructures and mechanical properties of AA7075 Al-5.7Zn-2.6Mg-1.5Cu-0.18Cr-0.08Mn-0.05Si-0.17Fe (wt.%) aluminum alloy have been investigated. The hardness of solution-treated samples (91.0 HV) profoundly increased to 146.8 HV after 7 days of natural ageing. The purpose of the present work was to examine the kinetic hardening evolution in subsequent artificial ageing treatments of samples naturally aged for 7 days and their counterparts without natural ageing. The former were labelled as NA-7d samples, and the latter, NA-0d samples. After artificial ageing at 120 degrees C for 2 h, the hardness of NA-0d samples increased rapidly to 148.2 HV, which was approximately the same as that of the specimens with natural ageing for 7 days, compensating for the prior state of lower hardness without natural ageing. After being treated at 120 degrees C for 16 h, the ultimate tensile strength (UTS) and yield strength (YS) of NA-7d reached the highest value, respectively, 601 MPa and 539 MPa, followed by a slight decrement of UTS when aged to 24 h. On the other hand, NA-0d specimens aged at 120 degrees C for 16 and 24 h showed nearly the same UTS (598 MPa); the former possessed YS of 538 MPa, and the latter, 545 MPa. The results presumably reveal that the peak ageing condition for NA-0d samples can be achieved under 24 h ageing at 120 degrees C. Under the same treatment at 120 degrees C for 24 h, the size of eta' phase in NA-7d sample (with a length of 4.96 nm) coarsened and grew larger than that in NA-0d sample (with a length of 3.46 nm). In addition, some eta' phase in the NA-7d sample was found to be transformed into the eta(2) them phase. The results indicated that the naturally aged specimens (NA-7d) reached the peak ageing condition earlier, but did not significantly enhance the UTS in AA7075 aluminum alloy, as compared to the samples without prior natural ageing (NA-0d). | en_US |
dc.language.iso | English | en_US |
dc.publisher | MDPI | en_US |
dc.relation.ispartof | METALS | en_US |
dc.subject | AA7075 aluminum alloys | en_US |
dc.subject | natural ageing | en_US |
dc.subject | eta ' and eta(2) phase | en_US |
dc.subject | mechanical properties | en_US |
dc.subject | high-resolution transmission electron microscopy | en_US |
dc.title | Effect of Natural Ageing on Subsequent Artificial Ageing of AA7075 Aluminum Alloy | en_US |
dc.type | journal article | en_US |
dc.identifier.doi | 10.3390/met12101766 | - |
dc.identifier.isi | WOS:000875256000001 | - |
dc.relation.journalvolume | 12 | en_US |
dc.relation.journalissue | 10 | en_US |
dc.identifier.eissn | 2075-4701 | - |
item.cerifentitytype | Publications | - |
item.openairetype | journal article | - |
item.openairecristype | http://purl.org/coar/resource_type/c_6501 | - |
item.fulltext | no fulltext | - |
item.grantfulltext | none | - |
item.languageiso639-1 | English | - |
crisitem.author.dept | College of Engineering | - |
crisitem.author.dept | Department of Mechanical and Mechatronic Engineering | - |
crisitem.author.dept | National Taiwan Ocean University,NTOU | - |
crisitem.author.parentorg | National Taiwan Ocean University,NTOU | - |
crisitem.author.parentorg | College of Engineering | - |
顯示於: | 機械與機電工程學系 |
在 IR 系統中的文件,除了特別指名其著作權條款之外,均受到著作權保護,並且保留所有的權利。