Title: | The oxidation behavior of an Fe61B15Zr8Mo7Co5Y2Cr2 bulk metallic glass at 550–700 °C | Authors: | Wu Kai Ren, I. F. Kao, P. C. Liu, C. T. Rong-Tan Huang |
Keywords: | B. Oxidation;B. Glasses, metallic | Issue Date: | Apr-2009 | Publisher: | Elsevier | Journal Volume: | 17 | Journal Issue: | 4 | Start page/Pages: | 205-210 | Source: | Intermetallics | Abstract: | The oxidation behavior of an Fe61B15Zr8Mo7Co5Y2Cr2 bulk metallic glass (Fe7-BMG) and its crystalline counterpart (XFe7) was studied over the temperature range of 550–700 °C in dry air. In general, the results showed that the oxidation kinetics of the Fe7-BMG and XFe7 alloys followed a parabolic-rate law, with their oxidation rates increasing with temperature. It was found that the oxidation rate constants (kp values) of the Fe7-BMG are slightly higher than those of XFe7, indicating that the amorphous alloy underwent a fast oxidation reaction. The scale formed on the Fe7-BMG at 550 °C for 48 h was thin and heterophasic mixture of iron oxides (Fe2O3/Fe3O4) and tetragonal-ZrO2 (t-ZrO2). At higher temperatures (T ≥ 600 °C), duplex scales formed on the glassy alloy consisted of an outer layer of iron oxides (Fe2O3/Fe3O4) and minor amounts of B2O3, and of a heterophasic inner layer of mostly t-ZrO2 intermixed with non-oxidized Fe3B, FeCo, and ZrB12. The formation of the crystalline intermetallics indicated the occurrence of the substrate crystallization at the temperature range of interest. |
URI: | http://scholars.ntou.edu.tw/handle/123456789/4479 | ISSN: | 0966-9795 | DOI: | 10.1016/j.intermet.2008.08.013 |
Appears in Collections: | 光電與材料科技學系 |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.