標題: Sulfide stress corrosion cracking and fatigue crack growth of welded TMCP API 5L X65 pipe-line steel
作者: LW Tsay 
YC Chen
Sammy Chan
公開日期: 二月-2001
卷: 23
期: 2
起(迄)頁: 103-113
來源出版物: International Journal of Fatigue
摘要: 
Slow strain rate tensile test and fatigue crack growth (FCG) test were performed to evaluate the fracture behavior of API 5L X65 steel weldments after hydrogen-charging. Regardless of the testing environments, tensile fracture of all welds was located at the weld metal (WM), which had the lowest hardness as compared to that of the other parts of the weld. When hydrogen-charged in an H 2S-saturated solution, all specimens suffered a small drop in tensile strength as compared to those tested in air; however, the loss in ductility was more significant. The susceptibility to hydrogen embrittlement of the welds could be reduced significantly by subjecting the welds to 600°C/2 h tempering treatment. With the tempering treatment, the number of surface cracks in the WM after hydrogen-charging decreased and the tensile properties improved. Results of FCG test demonstrated that in a higher stress intensity factor range (Δ K), tempered steel plates with a severely banding structure had the higher fatigue crack growth rates (FCGRs) than those of as-received ones. The WM of an uncharged weld had the lower FCGRs as compared to the parent metal within the same Δ K range. However, the enhancement of crack growth in the WM was very pronounced after hydrogen-charging. SEM fractographs of tensile and fatigue-fractured surfaces revealed a quasi-cleavage fracture in the embrittled region.
URI: http://scholars.ntou.edu.tw/handle/123456789/19934
DOI: 10.1016/S0142-1123(00)00081-5
顯示於:光電與材料科技學系

顯示文件完整紀錄

Page view(s)

78
上周
0
上個月
2
checked on 2025/6/30

Google ScholarTM

檢查

Altmetric

Altmetric

TAIR相關文章


在 IR 系統中的文件,除了特別指名其著作權條款之外,均受到著作權保護,並且保留所有的權利。

瀏覽
  • 機構典藏
  • 研究成果檢索
  • 研究人員
  • 單位
  • 計畫
DSpace-CRIS Software Copyright © 2002-  Duraspace   4science - Extension maintained and optimized by NTU Library Logo 4SCIENCE 回饋