Title: Oxidation Behavior of a Pd43Cu27Ni10P20 Bulk Metallic Glass and Foam in Dry Air
Authors: Wu Kai 
Ren, I. F.
Barnard, B.
Liaw, P. K.
Demetriou, M. D.
Johnson, W. L.
Keywords: Foam;Cu2O;Metallic Glass;Amorphous Alloy;Oxidation Kinetic
Issue Date: May-2010
Publisher: Springer Nature
Journal Volume: 41A
Journal Issue: 7
Start page/Pages: 1720–1725
Source: Metallurgical and Materials Transactions a-Physical Metallurgy and Materials Science
Abstract: 
The oxidation behavior of both Pd43Cu27Ni10P20 bulk metallic glass (Pd4-BMG) and its amorphous foam containing 45 pct porosity (Pd4-AF) was investigated over the temperature range of 343 K (70 °C) to 623 K (350 °C) in dry air. The results showed that virtually no oxidation occurred in the Pd4-BMG at T < 523 K (250 °C), revealing the alloy’s favorable oxidation resistance in this temperature range. In addition, the oxidation kinetics at T ≥ 523 K (250 °C) followed a parabolic-rate law, and the parabolic-rate constants (k p values) generally increased with temperature. It was found that the oxidation k p values of the Pd4-AF are slightly lower than those of the Pd4-BMG, indicating that the porous structure contributes to improving the overall oxidation resistance. The scale formed on the alloys was composed exclusively of CuO at T ≥ 548 K (275 °C), whose thickness gradually increased with increasing temperature. In addition, the amorphous structure remained unchanged at T ≤ 548 K (275 °C), while a triplex-phase structure developed after the oxidation at higher temperatures, consisting of Pd2Ni2P, Cu3P, and Pd3P.
URI: http://scholars.ntou.edu.tw/handle/123456789/4477
ISSN: 1073-5623
DOI: ://WOS:000277958700019
://WOS:000277958700019
://WOS:000277958700019
10.1007/s11661-010-0231-5
://WOS:000277958700019
://WOS:000277958700019
Appears in Collections:光電與材料科技學系

Show full item record

Page view(s)

303
Last Week
0
Last month
0
checked on Jun 30, 2025

Google ScholarTM

Check

Altmetric

Altmetric

Related Items in TAIR


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

Explore by
  • Communities & Collections
  • Research Outputs
  • Researchers
  • Organizations
  • Projects
Build with DSpace-CRIS - Extension maintained and optimized by Logo 4SCIENCE Feedback