標題: Microstructure and Stress Corrosion Cracking Behavior of the Weld Metal in Alloy 52-A508 Dissimilar Welds
作者: Wei-Chih Chung
Jiunn-Yuan Huang
Leu-Wen Tsay 
Chun Chen
關鍵字: A508 steel;Alloy 52 filler metal;dissimilar welds;microstructures;stress corrosion cracking;high-temperature water
公開日期: 一月-2011
卷: 52
期: 1
起(迄)頁: 12-19
來源出版物: Materials Transactions
摘要: 
In the nuclear power industry, dissimilar metal welding is widely used for joining low alloy steel to austenite stainless steel components with nickel-base filler metals. In this study, attention was paid to the weld metal in multi-pass Alloy 52-A508 dissimilar welds. An approximately 2 mm wide transition zone was observed that consisted of a martensitic layer (10∼20 um) along the weld interface and the austenite phase region with varying degrees of dilution. After post-weld heat treatment, the microstructures near the weld interface consisted of martensite, carbides and Type II boundaries. The presence of Type II boundaries significantly reduced the resistance to stress corrosion cracking (SCC) and formed intergranular cracking under simulated reactor coolant conditions. Constant extension rate tensile (CERT) tests were performed on the notched tensile specimens in 300°C water at two extension rates, 3×10−4 and 1×10−6 mm/s. A fast CERT test can be regarded to have no contribution of corrosion, and its results can be used as standards for comparison. In the slow CERT tests, the ductility losses of round-bar specimens with a circumferential notch at various regions in the weld metal were ranked accordingly. The relative susceptibility to SCC in terms of the ductility loss in increasing order of severity was as follows: the undiluted weld metal, the transition zone and the weld interface. SEM fractographic observations were consistent with the SCC results, i.e., an increased ductility loss or SCC susceptibility was associated with more brittle fractures.
URI: http://scholars.ntou.edu.tw/handle/123456789/4657
ISSN: 1345-9678
DOI: 10.2320/matertrans.M2010294
顯示於:光電與材料科技學系

顯示文件完整紀錄

WEB OF SCIENCETM
Citations

45
上周
1
上個月
1
checked on 2023/6/27

Page view(s)

106
上周
0
上個月
1
checked on 2025/6/30

Google ScholarTM

檢查

Altmetric

Altmetric

TAIR相關文章


在 IR 系統中的文件,除了特別指名其著作權條款之外,均受到著作權保護,並且保留所有的權利。

瀏覽
  • 機構典藏
  • 研究成果檢索
  • 研究人員
  • 單位
  • 計畫
DSpace-CRIS Software Copyright © 2002-  Duraspace   4science - Extension maintained and optimized by NTU Library Logo 4SCIENCE 回饋