標題: | High temperature corrosion behavior of iron aluminides containing ternary additions in H2/H2S/H2O mixed gases | 作者: | Chu, J. P. Pee-Yew Lee Wu Kai Rong-Tan Huang |
關鍵字: | High-temperature corrosion;Iron aluminides;Cr;Mn;Mo | 公開日期: | 十二月-1997 | 出版社: | Elsevier | 卷: | 239-240 | 起(迄)頁: | 859-870 | 來源出版物: | Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing | 摘要: | The high-temperature corrosion behavior of four iron aluminides containing Fe–18Al (in at.%) and three Fe–18Al–5M alloys (where M was Cr, Mn, or Mo) was studied over the temperature range of 700–900°C in a H2/H2S/H2O atmosphere. The corrosion kinetics followed the parabolic rate law in all cases, regardless of temperature and alloy composition. The parabolic rate constants decreased with decreasing temperature, and the addition of ternary elements resulted in various decreases in the corrosion rate compared with Fe–18Al. It was found that Mo was effective to improve the corrosion resistance at T≤800°C while Cr had a better improvement at 900°C. The scales formed on all iron aluminides were strongly dependent on temperature and ternary addition. |
URI: | http://scholars.ntou.edu.tw/handle/123456789/1893 | ISSN: | 0921-5093 | DOI: | 10.1016/s0921-5093(97)00676-x |
顯示於: | 光電與材料科技學系 |
在 IR 系統中的文件,除了特別指名其著作權條款之外,均受到著作權保護,並且保留所有的權利。