http://scholars.ntou.edu.tw/handle/123456789/4463
Title: | The corrosion behavior of Fe-Al alloys in H2/H2S/H2O atmospheres at 700–900°C | Authors: | Wu Kai Rong-Tan Huang |
Keywords: | corrosion;Fe-Al alloys;FeS;FeAl2S4;Al2O3 | Issue Date: | Aug-1997 | Publisher: | Springer Nature | Journal Volume: | 48 | Journal Issue: | 1-2 | Start page/Pages: | 59–86 | Source: | Oxidation of Metals | Abstract: | The corrosion behavior of five Fe-Al binary alloys containing up to 40 at. % Al was studied over the temperature range of 700–900°C in a H2/H2S/H2O mixture with varying sulfur partial pressures of 10−7−10−5 atm. and oxygen partial pressures of 10−24−10−2° atm. The corrosion kinetics followed the parabolic rate law in all cases, regardless of temperature and alloy composition. The parabolic rate constants decreased with increasing Al content. The scales formed on Fe-5 and −10 at.% Al were duplex, consisting of an outer layer of iron sulfide (FeS or Fe1−xS) and an inner complex scale of FeAl2S4 and FeS. Alloys having intermediate Al contents (Fe-18 and −28 at.% Al) formed scales that consisted of mostly iron sulfide and Al2O3 as well as minor a amount of FeAl2S4. The amount of Al2O3 increased with increasing Al content. The Fe 40 at.% Al formed only Al2O3 at 700°C, while most Al2O3 and some FeS were detected at T≥800°C. The formation of Al2O3 was responsible for the reduction of the corrosion rates. |
URI: | http://scholars.ntou.edu.tw/handle/123456789/4463 | ISSN: | 0030-770X | DOI: | 10.1007/bf01675262 |
Appears in Collections: | 光電與材料科技學系 |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.