標題: | The effect of post-weld heat treatment on the microstructure and notched tensile fracture of Ti-15V-3Cr-3Al-3Sn to Ti-6Al-4V dissimilar laser welds | 作者: | Hsieh, C. T. Shiue, R. K. Rong-Tan Huang Leu-Wen Tsay |
關鍵字: | Laser welding;Fusion zone;Notched tensile strength;Post-weld heat treatment;Ti–6–4;Ti–15–3 | 公開日期: | 一月-2016 | 卷: | 653 | 起(迄)頁: | 139-146 | 來源出版物: | Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing | 摘要: | A CO2 laser was applied for dissimilar welding of Ti–15V–3Cr–3Al–3Sn (Ti–15–3) to Ti–6Al–4V (Ti–6–4) alloys. The microstructures and notched tensile strength (NTS) of the dissimilar welds were investigated in the as-welded and post-weld heat treatment (PWHT) conditions, and the results were compared with Ti–6–4 and Ti–15–3 homogeneous laser welds with the same PWHT. The results indicated that predominant α″ with a few α and β phases was formed in the as-welded fusion zone (FZ). Furthermore, the FZ hardness was susceptible to the PWHT and showed a plateau for the specimens aged in the temperature range from 426 to 482 °C/4 h. In comparison with the homogeneous Ti–15–3 weld under the same PWHT conditions, the dilution of Ti–15–3 with Ti–6–4 caused a slight increase in the Al equivalent (AlEQ) of the FZ, resulting in a further rise in FZ hardness. With the PWHT at/below 538 °C, the dissimilar welds were associated with low NTS or high notch brittleness. |
URI: | http://scholars.ntou.edu.tw/handle/123456789/4570 | ISSN: | 0921-5093 | DOI: | 10.1016/j.msea.2015.12.013 |
顯示於: | 光電與材料科技學系 |
在 IR 系統中的文件,除了特別指名其著作權條款之外,均受到著作權保護,並且保留所有的權利。