標題: | Gaseous hydrogen embrittlement of T-250 laser welds | 作者: | L. W. Tsay W. B. Huang C. Chen |
關鍵字: | heat-affected zone;intergranular fracture;quasi-cleavage;weld metal | 公開日期: | 四月-1997 | 卷: | 6 | 期: | 2 | 起(迄)頁: | 182–186 | 來源出版物: | Journal of Materials Engineering and Performance | 摘要: | The tensile properties of laser-welded T-250 maraging steel are measured, with attention paid to the influence of strain rate and gaseous hydrogen on the fracture behavior of welded specimens. Post-weld heat treatments are performed on laser-welded specimens to obtain underaged (WU), peak-aged (WP), and overaged (WO) specimens. Hydrogen embrittlement (HE) affects the tensile fracture behavior of the welded specimens; HE changes not only the fracture mode but also the fracture location. Without the influence of hydrogen, the fracture location is at the softest region, the weld metal (WM), and the fracture appearance reveals a ductile dimple fracture. For welds sensitive to HE, the fracture is initiated at the heat-affected zone (HAZ) with coarse grain size, and the associated fracture surface exhibits intergranular and quasi-cleavage fractures that are brittle in nature. In addition, the HAZ with coarse grain size is more prone to HE, as compared to other regions in the welded specimens. The WU specimens are susceptible to HE in air under a low strain rate, while the WP specimens are only susceptible to gaseous hydrogen embrittlement (GHE). However, the WO specimens are immune to GHE and insensitive to strain rate. |
URI: | http://scholars.ntou.edu.tw/handle/123456789/4691 | ISSN: | 1059-9495 | DOI: | 10.1007/s11665-997-0012-5 |
顯示於: | 光電與材料科技學系 |
在 IR 系統中的文件,除了特別指名其著作權條款之外,均受到著作權保護,並且保留所有的權利。