Please use this identifier to cite or link to this item: http://scholars.ntou.edu.tw/handle/123456789/17477
Title: Microstructural Evolution of 9CrMoW Weld Metal in a Multiple-Pass Weld
Authors: Chuang, Yu-Lun
Wang, Chu-Chun
Chen, Tai-Cheng
Shiue, Ren-Kae
Tsay, Leu-Wen 
Keywords: 9CrMoW;weld metal;reheated microstructure;creep resistance
Issue Date: 1-Jun-2021
Publisher: MDPI
Journal Volume: 11
Journal Issue: 6
Source: METALS
Abstract: 
9CrMoW steel tubes were welded in multiple passes by gas-tungsten arc welding. The reheated microstructures in the Gr. 92 weld metal (WM) of a multiple-pass weld were simulated with an infrared heating system. Simulated specimens after tempering at 760 degrees C/2 h were subjected to constant load creep tests either at 630 degrees C/120 MPa or 660 degrees C/80 MPa. The simulated specimens were designated as the over-tempered (OT, below A(C1), i.e., WT-820T) and partially transformed (PT, below A(C3), i.e., WT-890T) samples. The transmission electron microscope (TEM) micrographs demonstrated that the tempered WM (WT) displayed coarse martensite packets with carbides along the lath and grain boundaries. Cellular subgrains and coarse carbides were observed in the WT-820T sample. A degraded lath morphology and numerous carbides in various dimensions were found in the WT-890T sample. The grain boundary map showed that the WT-820T sample had the same coarse-grained structure as the WT sample, but the WT-890T sample consisted of refined grains. The WT-890T samples with a fine-grained structure were more prone to creep fracture than the WT and WT-820T samples were. Intergranular cracking was more likely to occur at the corners of the crept samples, which suffered from high strain and stress concentration. As compared to the Gr. 91 steel or Gr. 91 WM, the Gr. 92 WM was more stable in maintaining its original microstructures under the same creep condition. Undegraded microstructures of the Gr. 92 WM strained at elevated temperatures were responsible for its higher resistance to creep failure during the practical service.
URI: http://scholars.ntou.edu.tw/handle/123456789/17477
DOI: 10.3390/met11060847
Appears in Collections:光電與材料科技學系

Show full item record

WEB OF SCIENCETM
Citations

1
Last Week
0
Last month
0
checked on Jun 27, 2023

Page view(s)

128
Last Week
0
Last month
0
checked on Jun 30, 2025

Google ScholarTM

Check

Altmetric

Altmetric

Related Items in TAIR


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

Explore by
  • Communities & Collections
  • Research Outputs
  • Researchers
  • Organizations
  • Projects
Build with DSpace-CRIS - Extension maintained and optimized by Logo 4SCIENCE Feedback