標題: Improving the Corrosion Resistance of 6061 Aluminum Alloy Using Anodization and Nickel-Cobalt based Sealing Treatment
作者: Lin, Ming-Yuan
Hsiao, Po-Sen
Sheu, Hung-Hua
Chang, Chin-Chun
Tsai, Ming-Shiun
Wuu, Dong-Sing
Lee, Hung-Bin 
關鍵字: 6061 aluminum alloy;nickel-cobalt sealing;corrosion resistance
公開日期: 1-十月-2021
出版社: ESG
卷: 16
期: 10
來源出版物: INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE
摘要: 
In this study, 6061 aluminum alloy was used as the substrate to form the oxide layer using room temperature and low temperature anodization treatment. The adhesion, corrosion resistance, micro structure, and mechanical properties of the oxide layer are studied. After anodization treatment, the hardness of the oxide layers are greater than 450 Hv, the highest hardness occurred at the oxide layer after nickel- cobalt sealing which hardness can reach 536 Hv. The thickness of the oxide layer formed by low temperature anodizing is about 45-50 mu m, and the thickness of the oxide layer formed by room temperature anodizing is only about 5-10 mu m. All aluminum anodization layers have contact angles above 60 degrees, and have high hardness, good hydrophobicity and high corrosion resistance. SEM, XPS, and TEM were used to analyze the chemical composition and microstructure of aluminum anodization layers prepared from different ratios of nickel and cobalt in the mixing solutions. The results show that when the ratio of nickel and cobalt is 8:2 in the mixing solutions, the aluminum anodization layer has the best sealing effect. When the substrates was carried out with anodization treatment and then sealed with the ratio of nickel- cobalt is 8:2, the lowest corrosion current density is 4.26 X 10(-9) A/cm(2). The corrosion current density of the substrates that was carried out with anodization treatment and then only sealed by boiling water is 3.55 X 10(-8) A/cm(2). When the substrates is only treated with anodization without sealing, its corrosion current density is only 5.8 X 10(-7) A/cm(2).
URI: http://scholars.ntou.edu.tw/handle/123456789/18213
ISSN: 1452-3981
DOI: 10.20964/2021.10.50
顯示於:光電與材料科技學系

顯示文件完整紀錄

WEB OF SCIENCETM
Citations

1
上周
0
上個月
1
checked on 2023/6/27

Page view(s)

298
上周
0
上個月
0
checked on 2025/6/30

Google ScholarTM

檢查

Altmetric

Altmetric

TAIR相關文章


在 IR 系統中的文件,除了特別指名其著作權條款之外,均受到著作權保護,並且保留所有的權利。

瀏覽
  • 機構典藏
  • 研究成果檢索
  • 研究人員
  • 單位
  • 計畫
DSpace-CRIS Software Copyright © 2002-  Duraspace   4science - Extension maintained and optimized by NTU Library Logo 4SCIENCE 回饋