Title: The Corrosion of Cu–Al Binary Alloys in H2/H2S/H2O Atmospheres at 400–900°C
Authors: Wu Kai 
Fan, G. W.
Chen, P. C.
Lin, Y. T.
Keywords: corrosion;Cu–Al alloys;Cu3Al;Cu9Al4;Cu2S;CuAlS2
Issue Date: Jun-2004
Publisher: Springer Nature
Journal Volume: 61
Journal Issue: 5-6
Start page/Pages: 439–461
Source: Oxidation of Metals
Abstract: 
The corrosion behavior of pure Cu and of three Cu–Al alloys containing 1, 5, and 10 wt.% Al was studied at 400–900°C in a H2/H2S/H2O gas mixture. Both Cu–1Al and Cu–5Al alloys had the single-phase structure of α-Cu, while Cu–10Al was the intermetallic compound Cu3Al. In general, the corrosion behavior of all the alloys followed the parabolic rate law, and the corrosion rate constants generally increased with increasing temperature but decreased with increasing Al content. The scale formed on pure Cu was an exclusive single layer of Cu2S, while the scales formed on Cu–Al alloys were heterophasic and duplex, consisting of an outer layer of Cu2S and an inner layer of Cu2S and CuAlS2. X-ray diffraction results showed no evidence of oxides and the amount of CuAlS2 increased with increasing Al content. The formation of Cu2S and CuAlS2 on higher Al-content alloys resulted in a subsurface phase transformation from α-Cu (for Cu–5Al) or from Cu3Al (for Cu–10Al) to Cu3Al + Cu9Al4. The formation of CuAlS2 in the inner layer of Cu–Al alloys was responsible for the reduction of corrosion rates, as compared to those of pure Cu.
URI: http://scholars.ntou.edu.tw/handle/123456789/4455
ISSN: 0030-770X
DOI: ://WOS:000222171800006
://WOS:000222171800006
://WOS:000222171800006
10.1023/B:OXID.0000032333.45244.c6
://WOS:000222171800006
://WOS:000222171800006
://WOS:000222171800006
://WOS:000222171800006
://WOS:000222171800006
Appears in Collections:光電與材料科技學系

Show full item record

Page view(s)

126
Last Week
0
Last month
0
checked on Jun 30, 2025

Google ScholarTM

Check

Altmetric

Altmetric

Related Items in TAIR


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

Explore by
  • Communities & Collections
  • Research Outputs
  • Researchers
  • Organizations
  • Projects
Build with DSpace-CRIS - Extension maintained and optimized by Logo 4SCIENCE Feedback