http://scholars.ntou.edu.tw/handle/123456789/4644
標題: | Stress corrosion cracking of austenitic weld deposits in a salt spray environment | 作者: | Cai, J. B. Yu, C. Shiue, R. K. Leu-Wen Tsay |
關鍵字: | Fusion zone;308L deposit;309LMo deposit;U-bend;Weight loss;Stress corrosion cracking | 公開日期: | 十月-2015 | 卷: | 465 | 起(迄)頁: | 774-783 | 來源出版物: | Journal of Nuclear Materials | 摘要: | ER 308L and 309LMo were utilized as the filler metals for the groove and overlay welds of a 304L stainless steel substrate, which was prepared via a gas tungsten arc-welding process in multiple passes. U-bend and weight-loss tests were conducted by testing the welds in a salt spray containing 10 wt% NaCl at 120 °C. The dissolution of the skeletal structure in the fusion zone (FZ) caused the stress corrosion cracking (SCC) of the weld. The FZ in the cold-rolled condition showed the longest single crack length in the U-bend tests. Moreover, sensitization treatment at 650 °C for 10 h promoted the formation of numerous fine cracks, which resulted in a high SCC susceptibility. The weight loss of the deposits was consistent with the SCC susceptibility of the welds in a salt spray. The 309LMo deposit was superior to the 308L deposit in the salt spray. |
URI: | http://scholars.ntou.edu.tw/handle/123456789/4644 | ISSN: | 0022-3115 | DOI: | 10.1016/j.jnucmat.2015.06.060 |
顯示於: | 光電與材料科技學系 |
在 IR 系統中的文件,除了特別指名其著作權條款之外,均受到著作權保護,並且保留所有的權利。