http://scholars.ntou.edu.tw/handle/123456789/4644
Title: | Stress corrosion cracking of austenitic weld deposits in a salt spray environment | Authors: | Cai, J. B. Yu, C. Shiue, R. K. Leu-Wen Tsay |
Keywords: | Fusion zone;308L deposit;309LMo deposit;U-bend;Weight loss;Stress corrosion cracking | Issue Date: | Oct-2015 | Journal Volume: | 465 | Start page/Pages: | 774-783 | Source: | Journal of Nuclear Materials | Abstract: | ER 308L and 309LMo were utilized as the filler metals for the groove and overlay welds of a 304L stainless steel substrate, which was prepared via a gas tungsten arc-welding process in multiple passes. U-bend and weight-loss tests were conducted by testing the welds in a salt spray containing 10 wt% NaCl at 120 °C. The dissolution of the skeletal structure in the fusion zone (FZ) caused the stress corrosion cracking (SCC) of the weld. The FZ in the cold-rolled condition showed the longest single crack length in the U-bend tests. Moreover, sensitization treatment at 650 °C for 10 h promoted the formation of numerous fine cracks, which resulted in a high SCC susceptibility. The weight loss of the deposits was consistent with the SCC susceptibility of the welds in a salt spray. The 309LMo deposit was superior to the 308L deposit in the salt spray. |
URI: | http://scholars.ntou.edu.tw/handle/123456789/4644 | ISSN: | 0022-3115 | DOI: | 10.1016/j.jnucmat.2015.06.060 |
Appears in Collections: | 光電與材料科技學系 |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.