標題: Stress corrosion cracking of austenitic weld deposits in a salt spray environment
作者: Cai, J. B.
Yu, C.
Shiue, R. K.
Leu-Wen Tsay 
關鍵字: Fusion zone;308L deposit;309LMo deposit;U-bend;Weight loss;Stress corrosion cracking
公開日期: 十月-2015
卷: 465
起(迄)頁: 774-783
來源出版物: Journal of Nuclear Materials
摘要: 
ER 308L and 309LMo were utilized as the filler metals for the groove and overlay welds of a 304L stainless steel substrate, which was prepared via a gas tungsten arc-welding process in multiple passes. U-bend and weight-loss tests were conducted by testing the welds in a salt spray containing 10 wt% NaCl at 120 °C. The dissolution of the skeletal structure in the fusion zone (FZ) caused the stress corrosion cracking (SCC) of the weld. The FZ in the cold-rolled condition showed the longest single crack length in the U-bend tests. Moreover, sensitization treatment at 650 °C for 10 h promoted the formation of numerous fine cracks, which resulted in a high SCC susceptibility. The weight loss of the deposits was consistent with the SCC susceptibility of the welds in a salt spray. The 309LMo deposit was superior to the 308L deposit in the salt spray.
URI: http://scholars.ntou.edu.tw/handle/123456789/4644
ISSN: 0022-3115
DOI: 10.1016/j.jnucmat.2015.06.060
顯示於:光電與材料科技學系

顯示文件完整紀錄

WEB OF SCIENCETM
Citations

13
上周
0
上個月
checked on 2023/5/7

Page view(s)

147
上周
0
上個月
0
checked on 2025/6/30

Google ScholarTM

檢查

Altmetric

Altmetric

TAIR相關文章


在 IR 系統中的文件,除了特別指名其著作權條款之外,均受到著作權保護,並且保留所有的權利。

瀏覽
  • 機構典藏
  • 研究成果檢索
  • 研究人員
  • 單位
  • 計畫
DSpace-CRIS Software Copyright © 2002-  Duraspace   4science - Extension maintained and optimized by NTU Library Logo 4SCIENCE 回饋